Thermal Spray Coating Performance Factors
Series 900
For Ferrous & Non-Ferrous Metals
Specific Performance Factors
- Endura® 900S
- Typical Surface Growth - 0.015"
- Hardness Equivalent - 90 Rc
- Non-Stick - Good
- Lubrication - N/A
- Non-Wetting - Good
- Corrosion / Chemical Resistance - Excellent
- Taber Abrasion Resistance - 0.01 g
- Max. Continious Operating Temperature - 2000°F
- FDA/USDA - Compliant
- Endura® 910
- Typical Surface Growth - 0.015"
- Hardness Equivalent - 50 Rc
- Non-Stick - Excellent
- Lubrication - Very Good
- Non-Wetting - N/A
- Corrosion / Chemical Resistance - Excellent
- Taber Abrasion Resistance - 0.01 g
- Max. Continious Operating Temperature - 500°F
- FDA/USDA - Compliant
- Endura® 931
- Typical Surface Growth - 0.015"
- Hardness Equivalent - 55 Rc
- Non-Stick - Excellent
- Lubrication - Very Good
- Non-Wetting - N/A
- Corrosion / Chemical Resistance - Excellent
- Taber Abrasion Resistance - 0.01 g
- Max. Continious Operating Temperature - 500°F
- FDA/USDA - Non-Compliant
- Endura® 948
- Typical Surface Growth - 0.015"
- Hardness Equivalent - 50 Rc
- Non-Stick - Excellent
- Lubrication - Very Good
- Non-Wetting - N/A
- Corrosion / Chemical Resistance - Very Good
- Taber Abrasion Resistance - 0.02 g
- Max. Continious Operating Temperature - 500°F
- FDA/USDA - Compliant
- Endura® 970
- Typical Surface Growth - 0.015"
- Hardness Equivalent - 50 Rc
- Non-Stick - Excellent
- Lubrication - Very Good
- Non-Wetting - N/A
- Corrosion / Chemical Resistance - Excellent
- Taber Abrasion Resistance - N/A
- Max. Continious Operating Temperature - 500°F
- FDA/USDA - Compliant
Please complete our Coating Requirement Questionnaire
or call us
at 1.800.336.3872 to review & discuss your project requirements.